Project Description
| Specification | Parameter |
|---|---|
| Size | 1-114 mm |
| Thickness | 0.2-20 mm |
| Color | Greyish White |
| Thermal Conductivity (1MHz) | 7±0.4 W/m·K |
| Thermal Conductivity (25°C) | ≥180 W/m·K |
| Bulk Density | ≥2.8 g/cm³ |
| Volume Resistivity | ≥10¹³ Ω·cm |
| Dielectric Loss Angle Tangent Value | ≤8×10⁻⁴ |
| Breakdown Strength | ≥20 kV/mm |
| Flexural Strength | ≥190 MPa |
| Operating Temperature | -40°C to +1200°C |
Application:
Beryllium Oxide Ceramic Plate, commonly referred to as Beryllia Plate, consists of BeO with 99% purity fabricated via controlled high-temperature processing. The material exhibits a density of at least 2.8 g/cm³ and a thermal conductivity of 180 W/m·K, which supports efficient heat dissipation in demanding thermal applications. Its high volume resistivity (≥10¹³ Ω·cm) makes it suitable for electrical insulation. Customizable dimensions further enable integration into various engineered systems.
Payment Terms: